      产品说明Product description
      一款高回弹性透明材料,具有极好的耐磨、耐高温性能。
       A kind of high resilience and translucent polymer material which has excellent wear resistance and high temperature resistance performance.

       

      关键特性Key characteristic
      1.耐老化性优良Excellent ageing resistance.
      2.表面哑,手感柔软干爽Dumb surface,soft and dry touch.
      3.模量高,不易变形High modulus,not easy to deformation.
      4.成型快,不粘模具Rapid molding,non-stick mold.
      5.可粘接材质:PP  Adhesive materials:PP.

       

      物理性能Physical properties结果 Result单位 Unit方法 Method
      硬度Hardness70±5shoreAASTM D2240
      熔融指数Melt indexgravity>2g/10minASTM D1238
      拉伸强度Tensile strength>8MpaASTM D412
      断裂延伸率Elongation at break>500%ASTM D412
      撕裂强度Tearing strengt>30Kn/mASTM D624
      比重Specific grav0.9±0.02g/cm3ASTM D792
      成型条件Molding condition


      干燥时间(Hour)Drying time2H螺筒一段温度(℃)Screw 1 temp 180℃
      干燥温度(℃)Drying temp 80℃螺筒二段温度(℃)Screw 2 temp 170℃
      射嘴温度(℃)Nozzle temp190℃螺筒三段温度(℃)Screw 3 temp 160℃



      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      谢运英:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:ES70B-KZ
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!